06233 872 300 info@cmc.de

What Weakens PEM Stacks— – How Modern Subframes Protect Against It

At the heart of every fuel cell is the Catalyst-Coated Membrane (CCM) – an extremely thin membrane coated with catalyst on both sides that enables charge transfer between the anode and cathode. To ensure that this delicate structure functions reliably, it must be mechanically supported, cleanly separated, and securely sealed. This is exactly where subframes and sealing adhesive films come into play.

The ion-exchange membrane – the heart of the PEM fuel cell

The membrane separates hydrogen and oxygen but allows protons to pass through. It is extremely thin, mechanically delicate, and is often built onto a reinforced or supported ePTFE structure. The catalyst layer consists of carbon and minute amounts of platinum (e.g., 0.1 mg/cm²).

The Most Important Damage Mechanisms in PEM Fuel Cells

Water Management

Too much or too little water damages the membrane:

• Flooding → Gas transport disrupted
• Drying out → Membrane loses conductivity

Causes: Imbalance between water production and consumption, poor gas diffusion.

Membran‑Degradation

The polymer membrane can be weakened by chemical and mechanical processes:

• oxidative radicals
• hydrolysis by water
• pressure and temperature fluctuations
• mechanical fatigue caused by swelling and drying out

Result: reduced proton conductivity → decrease in performance.

Corrosion

Metal components such as bipolar plates or current collectors can corrode:

• Contact with acidic media
• Electrochemical corrosion

Consequences: reduced conductivity, catalyst damage, structural defects.

Temperature gradients

Uneven temperatures cause thermal stresses:

• The stack heats up under load
• Insufficient cooling
• Localized hot spots

Result: mechanical damage to the diaphragm and components.

Catalyst Degradation

Catalysts can become “poisoned” or structurally damaged:

• Sulfur compounds, CO
• Metal cations
• Degradation products from gaskets, films, or adhesives
• Sintering at high temperatures
• Ostwald ripening
• Contaminants in the air stream

Consequence: a significant drop in performance, up to and including total failure.

Measures to Stabilize the Stack

  • Humidity Management Using Humidifiers

  • Thermal management to reduce thermal stress

  • Corrosion protection through coated bipolar plates

  • High-performance polymers for durable membranes

  • Reduced catalyst content due to smaller particle sizes (larger surface area, but more sensitive)

Catalyst poisoning caused by leached components

The MEA consists of several layers (bipolar plate, GDL, MPL, CCM, subframe). Each layer can release substances that:

• block catalysts
• reduce reactivity
• shorten service life

Particularly critical: hydrolysis at ~100°C and in polar media such as water.

Hydrolysis-Resistant Subframes & Sealing Films from CMC

To minimize these risks, CMC Klebetechnik offers the CMC 61145 adhesive film:

Properties:
• thin, electrically insulating
• specifically designed for high temperatures and polar media
• very high hydrolysis-stable adhesive strength
• resistant to solvents and deionized water (low pH)
• Good adhesion to ePTFE membranes
• Reliable sealing against crossover
Tests show: The special adhesive remains stable even under severe hydrolysis, solvents, and extremely acidic water.

Alternative films:
• PPS
• PEEK
• PVDF
→ Even higher hydrolysis stability possible.

Fazit

CMC 61145 is a high-performance solution for PEM fuel cells and PEM electrolysers. The film offers:

• high hydrolysis-stable adhesive strength
• resistance to polar media
• reliable sealing
• long service life

Ideal for demanding applications – such as electric buses, heavy-duty vehicles, or decentralized energy supply.